Acid proof brick main component is SiO2. When SiO2 is burned in high temperature, there are lots of polyaluminum andalusite which can resist acids strongly. Acid resistant brick also can resist alkali at room temperature because of high density, low water absorption. But it does not resist alkali at high temperature.

Acid Resistance, %:>99.8
Bulk Density, g/cm3:2.3-2.4
Water Absorption, %:≤0.5
Acid Proof Bricks

Acid Proof Bricks Overview

Acid proof brick main component is SiO2. When SiO2 is burned in high temperature, there are lots of polyaluminum andalusite which can resist acids strongly. Acid resistant brick also can resist alkali at room temperature because of high density, low water absorption. But it does not resist alkali at high temperature.

Features

  • High acid resistance, Low water absorption, Smooth furface, Precise size.
  • Anti-permeability, Anti-freeze, Salt resistance, Good adhesive property with other materials.
  • Can be installed on wet surface without drying, can get hardened under water or wet environment.
  • Easy to be installed, Easy to clean.
  • Can be customized according to customers’drawings.

Regular sizes
150*75*15/20/30mm
150*150*15/20/30mm
200*200*15/20/30mm
300*300*15/20/30mm

Standard sizes
230*113*15/20/30mm
230*113*40/50/60mm

All sizes brick can be made single side groove or double sides groove, glaze or non-glaze.
Special size and OEM service are provided, too.

Non Glaze: anti-skidding, anti-exposure.
Glaze: Easy to clean, smooth and clear.

Technical Specifications

Item Value
SiO2,% 60-70
Al2O3,% 20-30
FeO,% 0.5-3
Bulk Density, g/cm3 2.3-2.4
Acid Resistance, % >99.8
Water Absorption, % ≤0.5
Bending Strength, Mpa >58.8
Compressive Strength, Mpa ≥120

Industry Applications

Acid proof brick is widely used in chemical industry such as workshop, outdoor acid resistant floors, anti corrosion lining of tower, tank, sink, etc.

Proven Global Projects

Tai Wan Glass Group
Location China
Year 2020.12
Furnace Type Glass Kiln
Supplied Material Sintered AZS Brick
Zhuzhou Liling Kibing Glass Co., Ltd.
Location China
Year 2023.11
Furnace Type Glass Kiln
Supplied Material Zircon Bricks
Guangxi Xinfuxing Silicon Technology Co., Ltd.
Location China
Year 204.04
Furnace Type Glass Kiln
Supplied Material Sillimanite Bricks

About XZK Group

Strengths
Innovation
R&D Team
Facilities
Honors
Product Portfolio
Specializing in premium zircon, corundum, sintered AZS, and monolithics. With a $70M+ annual output, we deliver durable linings for global high-temp industries.
Capacity
✔ 4 automated microcomputer batching systems.
✔ 4 ultra-high-temp tunnel kilns & 5 shuttle kilns.
✔ 20+ CNC hydraulic presses (630-1500T).
✔ Digitalized workshops with 100,000T annual capacity.
Core Strengths
Core Strengths
Core Strengths
Core Strengths
Core Strengths
💡
93 patents, featuring the "Tri-Resist Brick" for glass kilns. Field-proven for superior corrosion and thermal shock resistance.
📜
Co-authored multiple National Standards for Andalusite, Chrome-Corundum, and Zircon bricks with CBMA.
🤝
Strategic partner to Fortune 500 leaders: China Baowu, CNBM, CSG, Xinyi, and Kibing Glass.
Tech & Innovation
Tech & Innovation
Tech & Innovation
Expert R&D Team
Led by Prof. Shi Gan, our 40+ engineers leverage advanced testing centers to drive innovation in green refractory technologies.
Professor Shi Gan
Prof. Shi Gan
Chief Scientist
Senior Engineer & National Expert (State Council Allowance).
Key drafter of 5+ national refractory standards.
Inventor of "Tri-Resist Brick", maximizing glass furnace lifespan.
R&D Center
Laboratory Equipment
Zhongke Refractories
Insulating Materials Base: Alumina Bubble, Mullite, High-Alumina & Fireclay bricks.
Zhongke New Materials
Special Refractories Base: Chrome-Corundum, Tri-Resist, and Low-Porosity bricks.
Henruida New Materials
Premium Refractories Base: Zircon, Corundum, Sintered AZS, and monolithics.
Zhengzhou Zhongke Refractories Co., Ltd. Zhengzhou Zhongke New Materials Co., Ltd. Zhengzhou Henruida New Materials Co., Ltd.
Certifications & Honors

Certified by ISO 9001, 14001, 45001, 50001 Management Systems.

Honored as:

  • National High-Tech Enterprise
  • Specialized & Innovative SME
  • Provincial Green Factory
  • Grade A Environmental Enterprise
Certifications & Honors
Beginning with professional consultation to accurately identify and address specific requirements
One-to-one Service
We offer one-on-one dedicated sales and technical team services to perfectly solve any refractory material problems you encounter
Professional Solution
The company has over 30 technical R&D personnel and can provide professional solutions based on the on-site conditions of customers
Quality Management System
We have a strict quality management system to ensure the stability of the quality of each batch of products.
Responsible After-sales Service
Our dedicated technical team will visit customers regularly and provide free lifetime after-sales service
leave a message for refractory
Contact Us
Phone/WhatsApp/Wechat: 0086 19059612888
Add: Micun & Laiji Refractory Industry Zone, Xinmi City, Henan Province, China
WhatsApp of XZK refractory WhatsApp
WeChat of XZK refractory WeChat
Leave a message
Please submit your inquiry using the form provided below. We will offer you a solution and quotation within 24 hours.

    CONTACT US
    To ensure we provide you with the best possible
    solution, please share:
    1. Type of refractory product you are interested in.
    2. Specific requirements (e.g., dimensions, quantity, using temp).
    3. Your industry or application area – this helps us
    tailor the ideal solution for you.
    Tel/WhatsApp/Wechat:
    0086 19059612888
    WhatsApp
    WeChat
    LEAVE A MESSAGE
    Please feel free to submit your inquiry using the form provided below, and we will provide you with a quote within 24 hours.

      WhatsApp

      WhatsApp ID: +86 190 5961 2888

      Email
      WeChat

      WeChat ID: +86 190 5961 2888

      Telephone